TY - JOUR
T1 - Thermophysical properties of Alloy 617 from 25°C to 1000°C
AU - Rabin, B. H.
AU - Swank, W. D.
AU - Wright, R. N.
N1 - Funding Information:
The authors would like to acknowledge D.C. Haggard for assistance in preparing specimens and Arnie Erickson for performing density measurements. This work was supported through the U.S. Department of Energy Nuclear Energy. Notwithstanding the terms and conditions included in this document, the identified paper, material, or work was or will be authored by Battelle Energy Alliance, LLC (BEA) under and is subject to Contract No. DE-AC07-05ID14517 with the U.S. Department of Energy taking priority. The United States Government retains, and the other entity or entities identified in this document, by accepting the identified paper, material, or work for publication acknowledges that the United States Government retains, a non-exclusive, paid-up, irrevocable, world-wide license to publish and reproduce the published form of the identified paper, material, or work or allow others to do so, for United States Government purposes. BEA does not make any expressed or implied representations or warranties, including, but not limited to, with respect to fitness for use of the identified paper, material, or work and BEA does not indemnify the other entity or entities identified in this document or any third parties from any and all claims, damages, or attorney fees that may arise from the use, reproduction, or publication of such paper, material, or work. Any and all litigation involving entities’ rights and duties under this document will be brought in a court of competent jurisdiction in the state (or equivalent) of the defendant's principal place of business identified in this document.
PY - 2013
Y1 - 2013
N2 - Key thermophysical properties needed for the successful design and use of Alloy 617 in steam generator and heat exchanger applications have been measured experimentally, and results are compared with literature values and results obtained from some other commercial Ni-Cr alloys and model materials. Specifically, the thermal diffusivity, thermal expansion coefficient, and specific heat capacity have been measured for Alloy 617 over a range of temperatures, allowing calculation of thermal conductivity up to 1000 C. It has been found that the thermal conductivity of Alloy 617 exhibits significant deviation from monotonic behavior in the temperature range from 600 C to 850 C, the temperatures of interest for most heat transfer applications. The non-linear behavior appears to result primarily from short-range order/disorder phenomena known to occur in the Ni-Cr system. Similar deviation from monotonic behavior was observed in the solid solution Ni-Cr-W Alloy 230, and lesser deviations were observed in iron based Alloy 800H and an austenitic stainless steel. Measured thermophysical property data are provided for four different heats of Alloy 617, and it is shown that property variations between the four different heats are not significant. Measurements were also obtained from Alloy 617 that was aged for up to 2000 h at 750 C, and it was found that this aging treatment does not significantly influence the thermophysical properties.
AB - Key thermophysical properties needed for the successful design and use of Alloy 617 in steam generator and heat exchanger applications have been measured experimentally, and results are compared with literature values and results obtained from some other commercial Ni-Cr alloys and model materials. Specifically, the thermal diffusivity, thermal expansion coefficient, and specific heat capacity have been measured for Alloy 617 over a range of temperatures, allowing calculation of thermal conductivity up to 1000 C. It has been found that the thermal conductivity of Alloy 617 exhibits significant deviation from monotonic behavior in the temperature range from 600 C to 850 C, the temperatures of interest for most heat transfer applications. The non-linear behavior appears to result primarily from short-range order/disorder phenomena known to occur in the Ni-Cr system. Similar deviation from monotonic behavior was observed in the solid solution Ni-Cr-W Alloy 230, and lesser deviations were observed in iron based Alloy 800H and an austenitic stainless steel. Measured thermophysical property data are provided for four different heats of Alloy 617, and it is shown that property variations between the four different heats are not significant. Measurements were also obtained from Alloy 617 that was aged for up to 2000 h at 750 C, and it was found that this aging treatment does not significantly influence the thermophysical properties.
KW - Alloy 617
KW - Thermal conductivity
KW - Thermophysical properties
UR - https://www.scopus.com/pages/publications/84877320261
U2 - 10.1016/j.nucengdes.2013.03.048
DO - 10.1016/j.nucengdes.2013.03.048
M3 - Article
AN - SCOPUS:84877320261
SN - 0029-5493
VL - 262
SP - 72
EP - 80
JO - Nuclear Engineering and Design
JF - Nuclear Engineering and Design
ER -