In this study, the stress corrosion cracking (SCC) of an Inconel Alloy 690 (UNS N06690) with a high percentage (26%) of cold work in two different deaerated high temperature waters, supercritical (above critical point) water (SCW) at 400°C and subcritical (below the critical point) water at 360°C, was studied by using tapered uniaxial tensile samples under constant load and U-bend samples under constant strain. The highly cold worked Alloy 690 tested is not representative and has a high density of TiN particles. This Alloy 690 is susceptible to stress corrosion cracking in SCW. The Alloy 690 tensile sample under 500MPa stress cracked significantly after exposure to SCW (400°C, 25MPa) for 696 hrs, but it did not crack after exposure to 360°C subcritical water under similar exposure duration and pressure. This shows supercritical water is more aggressive than subcritical water to initiate stress corrosion cracking. Generally, Alloy 690 has outstanding SCC performance in high temperature water. This unexpected poor SCC resistance in supercritical water is probably due to the much lower tensile ductility of this particular highly cold worked Alloy 690 and the unusual high density of TiN particles and their inhomogeneous distribution in the alloy. The strain level of the U-bend samples has significant effects on the stress corrosion cracking response. The U-bends with 10% strain cracked very severely in supercritical water, but the U-bends with a lower 6% strain did not crack in either supercritical or subcritical water.

Original languageEnglish
Title of host publicationNACE International - Corrosion Conference and Expo 2012
Pages4998-5007
Number of pages10
StatePublished - 2012
EventCorrosion 2012 - Salt Lake City, UT, United States
Duration: Mar 11 2012 → Mar 15 2012

Publication series

NameNACE - International Corrosion Conference Series
Volume6
ISSN (Print)0361-4409

Conference

ConferenceCorrosion 2012
Country/TerritoryUnited States
CitySalt Lake City, UT
Period03/11/12 → 03/15/12

Keywords

  • Alloy 690
  • Cold work
  • High temperature water
  • Stress corrosion cracking

Fingerprint

Dive into the research topics of 'Stress corrosion cracking of a highly cold worked INCONEL alloy 690 in deaerated high temperature water'. Together they form a unique fingerprint.

Cite this