Skip to main navigation Skip to search Skip to main content

Strain rate sensitivity of alloys 800H and 617

  • J. K. Wright
  • , J. A. Simpson
  • , R. N. Wright
  • , L. J. Carroll
  • , T. L. Sham

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review

10 Scopus citations

Abstract

The flow stress of many materials is a function of the applied strain rate at elevated temperature. The magnitude of this effect is captured by the strain rate sensitivity parameter "m". The strain rate sensitivity of two face-center cubic solid solution alloys that are proposed for use in high temperature heat exchanger or steam generator applications, Alloys 800H and 617, has been determined as a function of temperature over that range of temperatures relevant for these applications. In addition to determining the strain rate sensitivity, it is important for nuclear design within Section III of the ASME Boiler and Pressure Vessel Code to determine temperature below which the flow stress is not affected by the strain rate. This temperature has been determined for both Alloy 800H and Alloy 617. At high temperature the strain rate sensitivity of the two alloys is significant and they have similar m values. For Alloy 617 the temperature limit below which little or no strain rate sensitivity is observed is approximately 700°C. For Alloy 800H this temperature is approximately 650°C.

Original languageEnglish
Title of host publicationASME 2013 Pressure Vessels and Piping Conference, PVP 2013
DOIs
StatePublished - 2013
EventASME 2013 Pressure Vessels and Piping Conference, PVP 2013 - Paris, France
Duration: Jul 14 2013 → Jul 18 2013

Publication series

NameAmerican Society of Mechanical Engineers, Pressure Vessels and Piping Division (Publication) PVP
Volume1 A
ISSN (Print)0277-027X

Conference

ConferenceASME 2013 Pressure Vessels and Piping Conference, PVP 2013
Country/TerritoryFrance
CityParis
Period07/14/13 → 07/18/13

Fingerprint

Dive into the research topics of 'Strain rate sensitivity of alloys 800H and 617'. Together they form a unique fingerprint.

Cite this