Abstract
Ion irradiation experiments and atomistic simulations were used to demonstrate that irradiation-induced lattice swelling in a complex oxide, Lu 2Ti 2O 7, is due initially to the formation of cation antisite defects. X-ray diffraction revealed that cation antisite formation correlates directly with lattice swelling and indicates that the volume per antisite pair is approximately 12 Å 3. First principles calculations revealed that lattice swelling is best explained by cation antisite defects. Temperature accelerated dynamics simulations indicate that cation Frenkel defects are metastable and decay to form antisite defects.
| Original language | English |
|---|---|
| Article number | 195504 |
| Journal | Physical Review Letters |
| Volume | 108 |
| Issue number | 19 |
| DOIs | |
| State | Published - May 8 2012 |
Fingerprint
Dive into the research topics of 'Role of antisite disorder on preamorphization swelling in titanate pyrochlores'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver