Abstract

The oxidation behavior of Hf-Al-C ceramics containing 37.5 wt% Hf 3Al3C5, 30.5 wt%Hf2Al 4C5, and 32.0 wt% Hf3Al4C 6 has been investigated at 900°-1300°C in air. The oxidation kinetics approximately follows a linear law with the activation energy of 194±12 kJ/mol. The oxidation resistance of Hf-Al- C ceramics at high temperature is superior to HfC. The oxide scale is porous and composed of well-mixed t-HfO2 and Al2O3 as well as residual free carbon. The stabilization mechanisms of t-HfO2 and free carbon have been discussed. The simultaneous oxidation of Hf and Al in Hf-Al-C ceramics can be attributed to their close oxygen affinity as well as the strong coupling between Hf-C blocks and Al-C units in the crystal structures.

Original languageEnglish
Pages (from-to)3427-3431
Number of pages5
JournalJournal of the American Ceramic Society
Volume93
Issue number10
DOIs
StatePublished - Oct 2010

Fingerprint

Dive into the research topics of 'Oxidation behavior of ternary carbide ceramics in Hf-Al-C system in air'. Together they form a unique fingerprint.

Cite this