TY - JOUR
T1 - Modeling and validation of chemical vapor deposition of tungsten for tungsten fiber reinforced tungsten composites
AU - Raumann, L.
AU - Coenen, J. W.
AU - Riesch, J.
AU - Mao, Y.
AU - Gietl, H.
AU - Höschen, T.
AU - Linsmeier, Ch
AU - Guillon, O.
N1 - Funding Information:
This work has been carried out within the framework of the EUROfusion Consortium and has received funding from the Euratom research and training programme 2014–2018 and 2019–2020 under grant agreement No. 633053 . The views and opinions expressed herein do not necessarily reflect those of the European Commission.
Publisher Copyright:
© 2019 Elsevier B.V.
PY - 2020/1/15
Y1 - 2020/1/15
N2 - Tungsten is the most promising first wall material for nuclear fusion reactors. One disadvantage, however, is its intrinsic brittleness. Therefore, tungsten fiber reinforced tungsten (Wf/W) is developed for extrinsic toughening. Wf/W can be produced by chemical vapor deposition (CVD), e.g. by reducing WF6 with H2 using heated W-fibers as substrate. However, it still needs to be optimized regarding relative density and fiber volume fraction. The decisive factor is the tungsten deposition rate, which depends on the temperature and the partial pressures. For this dependence, however, there are controversial results in the literature. In this article, a new rate equation is presented, in which different literature equations are partially adapted and combined. It adjusts the WF6 reaction order between one and zero, depending on the temperature and the H2 and WF6 partial pressure. For validation, a simplified experimental setup with a single fiber was designed, which provides very well defined boundary conditions while varying the CVD process parameters heating temperature, pressure, gas flow rate and gas inlet composition. The experimental runs were simulated with COMSOL Multiphysics. The model was successfully validated by measurements of the WF6 consumption rates (< 2 to 100 %), deposited tungsten masses and spatially high-resolved tungsten deposition rates.
AB - Tungsten is the most promising first wall material for nuclear fusion reactors. One disadvantage, however, is its intrinsic brittleness. Therefore, tungsten fiber reinforced tungsten (Wf/W) is developed for extrinsic toughening. Wf/W can be produced by chemical vapor deposition (CVD), e.g. by reducing WF6 with H2 using heated W-fibers as substrate. However, it still needs to be optimized regarding relative density and fiber volume fraction. The decisive factor is the tungsten deposition rate, which depends on the temperature and the partial pressures. For this dependence, however, there are controversial results in the literature. In this article, a new rate equation is presented, in which different literature equations are partially adapted and combined. It adjusts the WF6 reaction order between one and zero, depending on the temperature and the H2 and WF6 partial pressure. For validation, a simplified experimental setup with a single fiber was designed, which provides very well defined boundary conditions while varying the CVD process parameters heating temperature, pressure, gas flow rate and gas inlet composition. The experimental runs were simulated with COMSOL Multiphysics. The model was successfully validated by measurements of the WF6 consumption rates (< 2 to 100 %), deposited tungsten masses and spatially high-resolved tungsten deposition rates.
KW - Chemical vapor deposition
KW - Comsol
KW - Experiment
KW - Modeling
KW - Rate equation
KW - Tungsten hexafluoride
UR - https://www.scopus.com/pages/publications/85076626065
UR - https://www.mendeley.com/catalogue/57861d9c-ded7-312a-b98e-454035a1030d/
U2 - 10.1016/j.surfcoat.2019.06.065
DO - 10.1016/j.surfcoat.2019.06.065
M3 - Article
AN - SCOPUS:85076626065
SN - 0257-8972
VL - 381
JO - Surface and Coatings Technology
JF - Surface and Coatings Technology
M1 - 124745
ER -