Mechanical properties of Au foams under nanoindentation

  • Carlos J. Ruestes
  • , Daniel Schwen
  • , Emmanuel N. Millán
  • , Emiliano Aparicio
  • , Eduardo M. Bringa

Research output: Contribution to journal › Article › peer-review

28 Scopus citations

Abstract

Nanoscale metallic foams display mechanical properties which make them attractive for a variety of technological applications. We report simulated nanoindentation tests for a model polycrystalline nanoporous gold structure with 11 nm mean filament diameter and 35 nm average grain size, comparable to foams produced by dealloying. Hardness, plasticity mechanisms, the extension of the plastic zone and the applicability of several scaling laws are discussed. Plasticity occurs at the nodes mainly and is dominated by nucleation of dislocations at the atomic steps of the ligament surfaces, in a dislocation accumulation scenario. Shockley partials, perfect dislocations, Hirth partials, Lomer-Cottrel locks and twins were identified. Grain boundary sliding appears to play a minor role in deformation at the indentation rates used. Several scaling laws are tested and their results and applicability are discussed based on the structural parameters of the foam and the deformation mechanisms identified.

Original languageEnglish
Pages (from-to)154-167
Number of pages14
JournalComputational Materials Science
Volume147
DOIs
StatePublished - May 2018

Keywords

  • Nanofoams
  • Nanoindentation
  • Plasticity
  • Simulation