TY - JOUR
T1 - In situ high-temperature 3D imaging of the damage evolution in a SiC nuclear fuel cladding material
AU - Yuan, Guanjie
AU - Forna-Kreutzer, J. Paul
AU - Xu, Peng
AU - Gonderman, Sean
AU - Deck, Christian
AU - Olson, Luke
AU - Lahoda, Edward
AU - Ritchie, Robert O.
AU - Liu, Dong
N1 - Funding Information:
D.L. acknowledges funding support from UK EPSRC ( EP/T000368/1 , EP/N004493/2 ). The authors also acknowledge the use of the X-ray synchrotron micro-tomography beamline (8.3.2) at the Lawrence Berkeley National Laboratory's Advanced Light Source, which is supported by the Office of Science of the U.S. Department of Energy under contract no. DE-AC02-05CH11231 . Thanks are also due to Dr. Dula Parkinson for help with these synchrotron tomography experiments.
Publisher Copyright:
© 2023 The Authors
PY - 2023/3
Y1 - 2023/3
N2 - Silicon carbide (SiC)-based nuclear fission fuel rod cladding has been considered as one of the possible designs for accident tolerant fuels. It is in the form of a SiC fibre reinforced SiC matrix composite tube (SiCf-SiCm) with monolithic SiC outer and/or inner coating layers. This study focuses on the deformation and fracture processes in this material using in situ X-ray micro-computed tomography (XCT) at room temperature (RT) and 1200 °C in an inert gas environment in a C-ring compression loading configuration. Prior to testing, local properties and residual stresses were characterised using nanoindentation and Raman spectroscopy since they can impact the mechanical behaviour of the material. The 3D strain distribution, crack formation and propagation processes including the toughening mechanisms (e.g., crack deflection, micro-cracking, crack bridging and bifurcation) are investigated in the coating and underlying composites at RT and 1200 °C. There is no particular sequence which toughening mechanism occurs first – this is very different from the conventional toughening theory in ceramic-matrix composites under uniaxial tension loading. Indeed, no evidence of fibre pull-out or fibre fracture was observed in this SiCf-SiCm nuclear cladding material in the current C-ring compression configuration. The correlation between local measurements and bulk mechanical behaviour are discussed.
AB - Silicon carbide (SiC)-based nuclear fission fuel rod cladding has been considered as one of the possible designs for accident tolerant fuels. It is in the form of a SiC fibre reinforced SiC matrix composite tube (SiCf-SiCm) with monolithic SiC outer and/or inner coating layers. This study focuses on the deformation and fracture processes in this material using in situ X-ray micro-computed tomography (XCT) at room temperature (RT) and 1200 °C in an inert gas environment in a C-ring compression loading configuration. Prior to testing, local properties and residual stresses were characterised using nanoindentation and Raman spectroscopy since they can impact the mechanical behaviour of the material. The 3D strain distribution, crack formation and propagation processes including the toughening mechanisms (e.g., crack deflection, micro-cracking, crack bridging and bifurcation) are investigated in the coating and underlying composites at RT and 1200 °C. There is no particular sequence which toughening mechanism occurs first – this is very different from the conventional toughening theory in ceramic-matrix composites under uniaxial tension loading. Indeed, no evidence of fibre pull-out or fibre fracture was observed in this SiCf-SiCm nuclear cladding material in the current C-ring compression configuration. The correlation between local measurements and bulk mechanical behaviour are discussed.
KW - C-ring compression
KW - Digital volume correlation
KW - SiC nuclear fuel cladding
KW - Toughening mechanisms
KW - X-ray computed micro-tomography
UR - https://www.scopus.com/pages/publications/85148875526
UR - https://www.mendeley.com/catalogue/4c581678-c0fe-3753-82d1-46a24cc69b0f/
U2 - 10.1016/j.matdes.2023.111784
DO - 10.1016/j.matdes.2023.111784
M3 - Article
AN - SCOPUS:85148875526
SN - 0264-1275
VL - 227
JO - Materials and Design
JF - Materials and Design
M1 - 111784
ER -