In-flight oxidation of aluminum in the twin-wire electric arc process

Research output: Contribution to journalReview articlepeer-review

18 Scopus citations

Abstract

This paper examines the in-flight oxidation of aluminum sprayed in air using the twin-wire electric are (TWEA) thermal spray process. Aerodynamic shear at the droplet surface increases the amount of in-flight oxidation by promoting entrainment of the surface oxides within the molten droplet and continually exposing fresh fluid available for oxidation. Mathematical predictions herein confirm experimental measurements that reveal an elevated, nearly constant surface temperature (∼2273 K) of the droplets during flight. The calculated oxide volume fraction of a "typical" droplet with internal circulation compares favorably to the experimentally determined oxide content (3.3-12.7%) for a typical TWEA-sprayed aluminum coating sprayed onto a room temperature substrate. It is concluded that internal circulation within the molten aluminum droplet is a significant source of oxidation. This effect produces an oxide content nearly two orders of magnitude larger than that of a droplet without continual oxidation.

Original languageEnglish
Pages (from-to)63-71
Number of pages9
JournalJournal of Thermal Spray Technology
Volume15
Issue number1
DOIs
StatePublished - Mar 2006

Keywords

  • Aluminum coatings
  • Oxidation
  • Twin-wire electric arc process