Abstract
An inexpensive, quick method has been developed to obtain uniform distributions of UO2 particles in a tungsten matrix utilizing 0.5 wt percent low density polyethylene. Powders were sintered in a Spark Plasma Sintering (SPS) furnace at 1600 °C, 1700 °C, 1750 °C, 1800 °C and 1850 °C using a modified sintering profile. This resulted in a uniform distribution of UO2 particles in a tungsten matrix with high densities, reaching 99.46% of theoretical for the sample sintered at 1850 °C. The powder process is described and the results of this study are given below.
| Original language | English |
|---|---|
| Pages (from-to) | 246-249 |
| Number of pages | 4 |
| Journal | Journal of Nuclear Materials |
| Volume | 486 |
| DOIs | |
| State | Published - Apr 1 2017 |
Keywords
- Density
- Nuclear Thermal Propulsion
- Spark plasma sintering
- Tungsten
- Uniform distribution
- Uranium dioxide
Fingerprint
Dive into the research topics of 'High density, uniformly distributed W/UO2 for use in Nuclear Thermal Propulsion'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver