TY - JOUR
T1 - Grain growth and mechanical properties of CeO2-x films deposited on Si(100) substrates by pulsed dc magnetron sputtering
AU - Park, In Wook
AU - Lin, Jianliang
AU - Moore, John J.
AU - Khafizov, Marat
AU - Hurley, David
AU - Manuel, Michele V.
AU - Allen, Todd
N1 - Funding Information:
This work was authored by a contractor of the U.S. Government under DOE Contract No. DE-AC07-05ID14517 , under the Energy Frontier Research Center (Office of Science, Office of Basic Energy Science, FWP 1356). Accordingly, the U.S. Government retains and the publisher, by accepting the article for publication, acknowledges that the U.S. Government retains a nonexclusive, paid-up, irrevocable, world-wide license to publish or reproduce the published form of this manuscript, or allow others to do so, for U.S. Government purposes.
PY - 2013/2/25
Y1 - 2013/2/25
N2 - CeO2-x films were deposited by sputtering a metal Ce target in a gas mixture of high purity Ar and O2 using a pulsed unbalanced magnetron sputtering system. In this work, cerium oxide thin films were grown onto silicon substrates under different O2 flow rates, which were varied from 20 to 80% of the total flow rate with simultaneous changes in the Ar flow rate. In addition, different growth conditions and the influence of post-deposition rapid thermal annealing (RTA) were performed to tailor the stoichiometry of the cerium oxide films. The microstructure and mechanical properties of the films were characterized using electron probe microanalysis (EPMA), X-ray diffraction, field-emission scanning electron microscopy, X-ray photoelectron spectroscopy, and nano-indentation. EPMA results revealed that all as-deposited CeO2-x films have an O/Ce ratio about 1.75. When the post-annealing temperature (TPA) for the films was increased from 800 to 1100°C, a reduction of oxygen in the film was observed, which led to a phase transition from cubic CeO2-x (111) to hexagonal Ce2O3 (002). This phase transition is related to Ce4+ to Ce3+ cation transformation due to the formation of oxygen vacancies. The hardness and elastic modulus of the as-deposited CeO2-x films were 11.7GPa and 241GPa, respectively, which were reduced to about 7.5GPa and 150GPa, respectively, after annealing at 1100°C.
AB - CeO2-x films were deposited by sputtering a metal Ce target in a gas mixture of high purity Ar and O2 using a pulsed unbalanced magnetron sputtering system. In this work, cerium oxide thin films were grown onto silicon substrates under different O2 flow rates, which were varied from 20 to 80% of the total flow rate with simultaneous changes in the Ar flow rate. In addition, different growth conditions and the influence of post-deposition rapid thermal annealing (RTA) were performed to tailor the stoichiometry of the cerium oxide films. The microstructure and mechanical properties of the films were characterized using electron probe microanalysis (EPMA), X-ray diffraction, field-emission scanning electron microscopy, X-ray photoelectron spectroscopy, and nano-indentation. EPMA results revealed that all as-deposited CeO2-x films have an O/Ce ratio about 1.75. When the post-annealing temperature (TPA) for the films was increased from 800 to 1100°C, a reduction of oxygen in the film was observed, which led to a phase transition from cubic CeO2-x (111) to hexagonal Ce2O3 (002). This phase transition is related to Ce4+ to Ce3+ cation transformation due to the formation of oxygen vacancies. The hardness and elastic modulus of the as-deposited CeO2-x films were 11.7GPa and 241GPa, respectively, which were reduced to about 7.5GPa and 150GPa, respectively, after annealing at 1100°C.
KW - CeO films
KW - Mechanical properties
KW - Phase transition
KW - Pulsed dc magnetron sputtering
KW - Rapid thermal annealing (RTA)
UR - https://www.scopus.com/pages/publications/84873250399
U2 - 10.1016/j.surfcoat.2012.11.068
DO - 10.1016/j.surfcoat.2012.11.068
M3 - Article
AN - SCOPUS:84873250399
SN - 0257-8972
VL - 217
SP - 34
EP - 38
JO - Surface and Coatings Technology
JF - Surface and Coatings Technology
ER -