TY - JOUR
T1 - Evolution of manganese-nickel-silicon-dominated phases in highly irradiated reactor pressure vessel steels
AU - Wells, Peter B.
AU - Yamamoto, Takuya
AU - Miller, Brandon
AU - Milot, Tim
AU - Cole, James
AU - Wu, Yuan
AU - Odette, G. Robert
N1 - Funding Information:
A portion of this research, both the ATR irradiation and FIB/APT at the Center for Advanced Energy Studies—Microscopy and Characterization Suite (CAES-MaCS), was supported by the Advanced Test Reactor National Scientific User Facility through the US Department of Energy, Office of Nuclear Energy under DOE Idaho Operations Office Contract DE-AC07-051D14517. Special thanks go to Colin Knight at the Idaho National Laboratory for assisting in the complex steps needed to gain access to the irradiated ATR specimens. The much earlier piggyback BR2 irradiations were sponsored by Jean Claude Van Duysen of Electricité de France and carried out under the supervision of Lorenzo Malerbra at SCK Belgium. We also thank Peter Hosemann at UC Berkeley for access to their FIB to prepare APT samples from the high-fluence (BR2) condition. The MRL Shared Experimental Facilities were used for performing APT on the high-fluence (BR2) samples and are supported by the MRSEC Program of the NSF under Award No. DMR 1121053 as a member of the NSF-funded Materials Research Facilities Network (www.mrfn.org). The bulk of this research was supported by the DOE Office of Nuclear Energy’s Nuclear Energy University Program, as part of the LRW Sustainability Task. Finally we thank Huibin Ke, Professor Dane Morgan and our other collaborators at the University of Wisconsin who are leading the modeling effort cited in this paper and who were the source of many helpful discussions and much insight.
PY - 2014/11
Y1 - 2014/11
N2 - Formation of a high density of Mn-Ni-Si nanoscale precipitates in irradiated Cu-free and Cu-bearing reactor pressure vessel steels could lead to severe unexpected embrittlement. Models long ago predicted that these precipitates, which are not treated in current embrittlement prediction models, would emerge only at high fluence. However, the mechanisms and variables that control Mn-Ni-Si precipitate formation, and their detailed characteristics, have not been well understood. High flux irradiations of six steels with systematic variations in Cu and Ni contents were carried out at ∼295 °C to high and very high neutron fluences of ∼1.3 × 1020 and ∼1.1 × 1021 n cm-2. Atom probe tomography shows that significant mole fractions of Mn-Ni-Si-dominated precipitates form in the Cu-bearing steels at ∼1.3 × 1020 n cm-2, while they are only beginning to develop in Cu-free steels. However, large mole fractions of these precipitates, far in excess of those found in previous studies, are observed at 1.1 × 1021 n cm-2 at all Cu contents. At the highest fluence, the precipitate mole fractions primarily depend on the alloy Ni, rather than Cu, content. The Mn-Ni-Si precipitates lead to very large increases in measured hardness, corresponding to yield strength elevations of up to almost 700 MPa.
AB - Formation of a high density of Mn-Ni-Si nanoscale precipitates in irradiated Cu-free and Cu-bearing reactor pressure vessel steels could lead to severe unexpected embrittlement. Models long ago predicted that these precipitates, which are not treated in current embrittlement prediction models, would emerge only at high fluence. However, the mechanisms and variables that control Mn-Ni-Si precipitate formation, and their detailed characteristics, have not been well understood. High flux irradiations of six steels with systematic variations in Cu and Ni contents were carried out at ∼295 °C to high and very high neutron fluences of ∼1.3 × 1020 and ∼1.1 × 1021 n cm-2. Atom probe tomography shows that significant mole fractions of Mn-Ni-Si-dominated precipitates form in the Cu-bearing steels at ∼1.3 × 1020 n cm-2, while they are only beginning to develop in Cu-free steels. However, large mole fractions of these precipitates, far in excess of those found in previous studies, are observed at 1.1 × 1021 n cm-2 at all Cu contents. At the highest fluence, the precipitate mole fractions primarily depend on the alloy Ni, rather than Cu, content. The Mn-Ni-Si precipitates lead to very large increases in measured hardness, corresponding to yield strength elevations of up to almost 700 MPa.
KW - Atom probe tomography
KW - Irradiation embrittlement
KW - Precipitation
KW - Radiation damage
UR - https://www.scopus.com/pages/publications/84906703111
U2 - 10.1016/j.actamat.2014.07.040
DO - 10.1016/j.actamat.2014.07.040
M3 - Article
AN - SCOPUS:84906703111
SN - 1359-6454
VL - 80
SP - 205
EP - 219
JO - Acta Materialia
JF - Acta Materialia
ER -