Abstract
Elevated temperature tensile and creep-rupture tests were performed on INCONEL alloy MA754 in an as-rolled, fine-grained condition. Tensile tests were performed at 25 °C, 800 °C, 900 °C, and 1000 °C; creep-rupture tests were performed at 800 °C, 900 °C, and 1000 °C. The elevated temperature strength in the fine-grained condition was approximately 25 pct of that in the coarse-grained, annealed condition. While good ductility was observed in tensile tests at a nominal strain rate of 1 × 10-3 s-1, ductility in creep-rupture tests was very low, with failure elongations less than 5 pct and no reduction in area. Creep deformation appeared to occur primarily by cavity formation and growth.
| Original language | English |
|---|---|
| Pages (from-to) | 2552-2555 |
| Number of pages | 4 |
| Journal | Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science |
| Volume | 36 |
| Issue number | 9 |
| DOIs | |
| State | Published - Sep 2005 |
Fingerprint
Dive into the research topics of 'Elevated temperature strength of fine-grained INCONEL alloy MA754'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver