Abstract
Elemental powder mixture of Fe-Cr-Ti-Mo and La2O3 were ball milled for different milling times in a high energy shaker mill. Effects of ball milling time on crystallite size, particle size and hardness were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM) and microhardness tester. After 10 h of ball milling, the smallest crystallite size and highest hardness were ∼24 nm and ∼970 HV, respectively. Transmission electron microscopy (TEM) studies have revealed nanoscale features 2-5 nm in diameter present in the milled powder. Local atom probe tomography studies have shown that these nanoscale features were possibly nanoclusters enriched in La, TiO and O.
| Original language | English |
|---|---|
| Pages (from-to) | 282-286 |
| Number of pages | 5 |
| Journal | Journal of Nuclear Materials |
| Volume | 434 |
| Issue number | 1-3 |
| DOIs | |
| State | Published - 2013 |
Fingerprint
Dive into the research topics of 'A preliminary study on the development of La2O 3-bearing nanostructured ferritic steels via high energy ball milling'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver